In the production process, because pp fitting is a heat sensitive material, even adding heat stabilizer can only increase the decomposition temperature, and extend the stability time without decomposition, which requires that the molding and processing temperature of PP should be strictly controlled.

1. Temperature control
Temperature control is an important control factor in extrusion operation. The temperature of the control factors needed for extrusion is barrel temperature, diameter temperature and die temperature. The temperature is too low, the plasticization is not good, the appearance of the pipe is not glossy, the mechanical properties are poor, the product quality can not meet the requirements: the temperature is too high, the material will decompose, the product discoloration and other phenomena appear.

2. Screw speed
With the increase of screw rotation speed, the extrusion volume will increase, so the output can be increased, but it is easy to produce the phenomenon of poor plasticization, resulting in the roughness of the inner wall of the pipe and the decrease of the strength. At this time, the head pressure should be adjusted to achieve the best output and quality. The temperature control of screw affects the conveying rate, plasticization and melting quality of materials. The extrusion pipe needs cooling water to reduce the screw temperature, which is conducive to improving the plasticizing quality. The screw cooling water temperature is about 50 ~ 70.

3. Traction speed
In the re extrusion operation, it is very important to adjust the traction speed. After extrusion, melting and plasticizing, the material is drawn after continuous extrusion from the head, thus entering the setting device, cooling device, traction device, etc. the traction speed should match the extrusion speed. Generally, in normal production, the pulling speed should be about 1% ~ 10% faster than the extrusion speed of pipe.

4. Compressed air and pressure
Compressed air can blow the pipe and keep the pipe roundness. It is required that the pressure should be appropriate. The pressure is too small, the pipe is not round, the pressure is too large, the core mold is cooled, the inner wall of the pipe cracks, is not smooth, and the quality of the pipe decreases. At the same time, the pressure is required to be stable. For example, the pressure varies from big to small, and the pipe is prone to produce the status quo of slub.

5. Temperature of sizing device and cooling device